[TheForge] Manual shears and punches

Ries Niemi rniemi at fidalgo.net
Fri Mar 11 20:13:23 EST 2005


On Friday, March 11, 2005, at 04:09 PM, xlch58 at swbell.net wrote:

> Harbor Freight used to sell a chinese copy.  I bought one years ago 
> and it does fine with quarter inch plate.  Where it really shines ( vs 
> the other options I have) is for expanded metal.  Beats plasma, oxygen 
> etc.   It cost me $89 on sale about ten years ago.
>
> Charles
>
>

Yeah, but the harbor freight doesnt have little shear spots for 
shearing round, square, angle, and punching as well, like the old 
buffalo's and the new german ones. It is just a straight shear, nada 
mas.

ries



More information about the TheForge mailing list