Dan, Nah, no war; but isn't "Scrounging 101" in the curriculum of one of ur
demos? Ron C
-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net] On Behalf Of Dan Tull
Sent: Wednesday, April 20, 2005 10:54 AM
To: Sponsored by ABANA
Subject: Re: [TheForge] Super Quenched Dies?
I detect a flame war brewing.
Maybe you should change your priorties then. There is plenty of tool steel
available free if you will "lower" yourself enough to ask.
But then you probably wouldn't go dumpster diving either, huh.?
----- Original Message -----
From: "Chris Kilpatrick" <crimsonkil at lycos.com>
To: <munlaw2 at hcsmail.com>; "Sponsored by ABANA" <theforge at mailman.qth.net>
Sent: Wednesday, April 20, 2005 10:47 AM
Subject: RE: [TheForge] Super Quenched Dies?
Rob gunther got a 48 rockwell all the way through a 1" bar, I'd say the
quench goes pretty deep. there are some of us here who have a forging
budget of about $25/week, because it is a hobby, so 'good steel lying
around' does not describe my shop.
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
password: anvil
___________
More information about the TheForge
mailing list