[TheForge] Super Quenched Dies?
Ron Childers
munlaw2 at hcsmail.com
Wed Apr 20 10:22:59 EDT 2005
It won't harden all the way through and the dies won't last as long as high
carbon steel. With all the good steel "laying around", why waste time & $$
on something with which you will not be happy? Even the dies that come with
the larger hammers have to be dressed periodically. Specialty dies will
probably work ok for a while, but dies used every day in a production
setting would deform.
Ron C
-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net] On Behalf Of schade at acegroup.cc
Sent: Wednesday, April 20, 2005 9:33 AM
To: Sponsored by ABANA; munlaw2 at hcsmail.com
Subject: Re: [TheForge] Super Quenched Dies?
On Apr 20, 2005, at 7:20 AM, Ron Childers wrote:
> Echo Dan: *Don't*
>
>
Why not?