That's the main thing I noticed in my forge- the reflected heat. I
already had Durablanket (?) for the inside layer of insulation, which is
a huge improvement on Kaowool, but a coating of Plistix must have bumped
the top end up a couple hundred degrees. Forge weld like crazy...
Andy G.
_______________________________________________
Andy G.
Could you please explain to me what you mean by "a huge improvement on
Kaowool." Not that I'm arguing the point; I don't have stock in either manufacturer.
Mike P.