[TheForge] local source of ITC 100

Michael Horgan lughaid at earthlink.net
Sun Apr 3 11:12:01 EDT 2005


Welcome back, Mikey.
At 09:36 PM 4/2/2005, you wrote:

>I don't really know how well Plistix 900F reflects IR, but it certainly makes
>a terrific seal coating; far superior to ITC #100. They aren't even in the
>same league. I will be using the Plistix on a new miniature Multihole furnace
>shortly and then I will know whether to bother using water separated #200 
>mesh
>Zirconia over the Plistix or not.
>Michael Porter

Michael D. Horgan , lughaid at earthlink.net
http://members.aol.com/lughaid/
posting from
  A BRAZEN FORGERY
Blacksmithing and Metalwork
Claremont, Ca.