Catherine Jo:  What a great idea re the crock pot.  Much safer than the open
flame.
The rags also may spontaneously combust if kept in a closed container.

                                        Grant Marcoux
----- Original Message -----
From: "Catherine Jo Morgan" <[email protected]>
To: "'Blacksmithing mailing list'" <[email protected]>
Sent: Wednesday, April 16, 2003 9:25 AM
Subject: [TheForge] oil-wax finish


> I used the oil-wax-turpentine finish for quite a few years. Added a tiny
> bit of cobalt drier to it. One of those $10 mini crockpots works well to
> heat it, including for the initial mix. Then you just store it in the
> crockpot and plug it in when you get ready to finish. This is safe
> compared with heating it over an open flame.
>
> Be careful of those rags afterwards. That's a big fire hazard with this
> finish.
>
> Catherine Jo Morgan
> Morgan Sculpture
> Iron and mixed media vessels
> [email protected]
> 706-754-3812
>
> online artist journal: http://radio.weblogs.com/0120691/
>
>
>
> --- StripMime Report -- processed MIME parts ---
> multipart/alternative
>   text/plain (text body -- kept)
>   text/html
> The reason this message is shown is because the post was in HTML
> or had an attachment.  Attachments are not allowed.  To learn how
> to post in Plain-Text go to: http://www.expita.com/nomime.html  ---
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  [email protected]
> password:  anvil
> ___________
>
>
>