[TheForge] Hammer Anvil Materials
Ralph Sproul
[email protected]
Mon Apr 7 20:32:00 2003
Bob, That first shaft came of a chipper.......the frame is still
down back. :-)
Ralph
----- Original Message -----
From: <[email protected]>
To: <[email protected]>
Sent: Monday, April 07, 2003 7:45 PM
Subject: Re: [TheForge] Hammer Anvil Materials
> My small air hammer has a 4.5" dia solid anvil.I got it as scrap from a
piece
> of machinery.Can't remember what it was though but it sure does work
good.The
> smaller bench hammer has a 4.5" dia hollow but 1" thick wall with a piece
of
> 3" thick 5.5" dia 4140 welded to the top as the anvil.Both seem to be very
> effective
>
> Bob
> HotAnvil Forge
> http://members.tripod.com/hotanvil_forge
>
>
> --- StripMime Report -- processed MIME parts ---
> multipart/alternative
> text/plain (text body -- kept)
> text/html
> The reason this message is shown is because the post was in HTML
> or had an attachment. Attachments are not allowed. To learn how
> to post in Plain-Text go to: http://www.expita.com/nomime.html ---
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: [email protected]
> password: anvil
> ___________
>
>