My small air hammer has a 4.5" dia solid anvil.I got it as scrap from a piece
of machinery.Can't remember what it was though but it sure does work good.The
smaller bench hammer has a 4.5" dia hollow but 1" thick wall with a piece of
3" thick 5.5" dia 4140 welded to the top as the anvil.Both seem to be very
effective
Bob