Hi Group
Its been awhile. Did ya miss me.?
I have a problem I would appreciate some input on. We are welding a trailer
hitch. major heavy duty. F450
quarter inch plate. welding at a 90 degree right angle. we are starting at
the center and working out. as indicated by the red arrows.
The part is warping in direction of the blue arrows. only about 3/19 th on
each end but this is enough that on the next part marriage the part rocks
and does not fit flush against the next part. customer is adamant that it
must.
Anyone have any ideas ?
I'm thinking the direction matters. or at lease tack the two ends and then
weld from the center out.
Thanks in advance
Hope all is well with your and yours.
Marc Davis
Maui Pirate Association
Marc of the Hammer
Maui Marckey on FB
313 205 2855
MPA at marc3rd.com
______________________________________________________________
TheForge mailing list
Home: http://mailman.qth.net/mailman/listinfo/theforge
Help: http://mailman.qth.net/mmfaq.htm
Post: mailto:TheForge at mailman.qth.net
TheForge mail list group photo site is
http://www.shutterfly.com
Login: blacksmithblacksmith at hotmail.com
Password: anvil
This list hosted by: http://www.qsl.net
Please help support this email list: http://www.qsl.net/donate.html
More information about the TheForge
mailing list