Well a obviously it is the blue arrows, that’s why I only use high quality red arrows;’)

Pictures don’t come through on the forge, so you are going to have to paint a picture with words..

Charles

Sent from my iPad

> On Jan 24, 2019, at 1:48 PM, <Marc3rd at marc3rd.com> <Marc3rd at marc3rd.com> wrote:
> 
> Hi Group
> Its been awhile. Did ya miss me.?
> 
> I have a problem I would appreciate some input on. We are welding a trailer hitch. major heavy duty. F450
> 
> quarter inch plate. welding at a 90 degree right angle. we are starting at the center and working out. as indicated by the red arrows.
> 
> The part is warping in direction of the blue arrows. only about 3/19 th on each end but this is enough that on the next part marriage the part rocks and does not fit flush against the next part. customer is adamant  that it must.
> 
> Anyone have any ideas ?
> 
> I'm thinking the direction matters. or at lease tack the two ends and then weld from the center out.
> Thanks in advance
> Hope all is well with your and yours.
> 
> Marc Davis
> Maui Pirate Association
> Marc of the Hammer
> Maui Marckey on FB
> 313 205 2855
> MPA at marc3rd.com 
> 
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
> 
> TheForge mail list group photo site is
> http://www.shutterfly.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
> 
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html



More information about the TheForge mailing list