Bill what I use is just some clay i got from a building site for a
house it was blue clay but the red clay works to I put about 1 1/2 on
it and has been there for years when cracked i just work some more in to
the cracks
On 10/25/2017 8:18 AM, bilcol wrote:
> Thanks Mike. I never coated the forge with a refractory material but maybe
> I should have. Since the pan has not burned/rusted through yet I might want
> to try adding a layer of a castable or rammable refractory before
> reinforcing the steel bottom. Do you know how thick the coating should be
> on this type of forge? And, do you know what type of material might hold up
> best to wear and flux?
>
> Bill
>
> -----Original Message-----
> From: theforge-bounces at mailman.qth.net
> [mailto:theforge-bounces at mailman.qth.net] On Behalf Of Michael via TheForge
> Sent: Tuesday, October 24, 2017 4:11 PM
> To: theforge at mailman.qth.net
> Subject: Re: [TheForge] forge repair
>
> those small rivet forges need to be sealed/coated with fire clay every so
> often. you can buy it at a refractory outlet for cheap money.
> regards,
> Mike Schermerhorn
> Boston
>
>
>
> -----Original Message-----
> From: J. Petrila <jlpservicesinc at gmail.com>
> To: Blacksmithing List Sponsored by A/coANA <theforge at mailman.qth.net>
> Sent: Sat, Oct 21, 2017 12:15 pm
> Subject: Re: [TheForge] forge repair
>
> Using a large disk of steel would work great.. lea 've it loose in the
> forge bed with nothing in it but the firepot. This will allow for the
> items to expand and contract at different rates..
>
> On Oct 21, 2017 11:54 AM, "bilcol" <bilcol at bohlfamily.com> wrote:
>
>> I have a rivet forge that has worked well over the years but after
>> cleaning it out recently I see that the bottom of the pan is in bad
>> shape. Due to rust (in south Florida) and use, much of it is getting
>> fairly thin so I am concerned that it could burn through soon. There
>> is also at least one through crack. So I need to reinforce it
>> somehow. I am considering using a donut shaped steel disk that would
>> cover the region between the outer rim and the tuyere but wonder
>> whether a packed refractory could do the job or if there might be
>> another solution. Any comments/suggestions would be appreciated.
>>
>>
>>
>> Bill
>>
>>
>>
>>
>>
>> Bill and Colette
>>
>> bilcol at bohlfamily.com <mailto:bilcol at bohlfamily.com>
>>
>> www.bohlfamily.com <http://www.bohlfamily.com>
>>
>>
>>
>> ______________________________________________________________
>> TheForge mailing list
>> Home: http://mailman.qth.net/mailman/listinfo/theforge
>> Help: http://mailman.qth.net/mmfaq.htm
>> Post: mailto:TheForge at mailman.qth.net
>>
>> TheForge mail list group photo site is http://www.shutterfly.com
>> Login: blacksmithblacksmith at hotmail.com
>> Password: anvil
>>
>> This list hosted by: http://www.qsl.net Please help support this email
>> list: http://www.qsl.net/donate.html
>>
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.shutterfly.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
>
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.shutterfly.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
>
>
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.shutterfly.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
More information about the TheForge
mailing list