[TheForge] Old band saw blade

Dave Smucker davesmucker at hotmail.com
Mon Aug 14 17:19:11 EDT 2017


Google - D6A steel -  that is some damn strong steel.  (not cheap to make also)  Thanks Michael.

Dave Smucker
Brasstown, NC

-----Original Message-----
From: theforge-bounces at mailman.qth.net [mailto:theforge-bounces at mailman.qth.net] On Behalf Of Michael via TheForge
Sent: Monday, August 14, 2017 3:06 PM
To: theforge at mailman.qth.net
Subject: Re: [TheForge] Old band saw blade


the material used for blades that have carbide teeth eb welded to it is D6A.
Michael Schermerhorn
Boston



-----Original Message-----
From: Dave Smucker <davesmucker at hotmail.com>
To: Blacksmithing List Sponsored by ABANA <theforge at mailman.qth.net>
Sent: Mon, Aug 14, 2017 11:38 am
Subject: Re: [TheForge] Old band saw blade

For those of you that may not know - L6 is basically  - 4370  -  like 4340 but with 70 points of carbon instead of 40.  Very good steel and you can heat-treat it just like it was 4140 or 4340 but it will be harder.  Don't forget to temper. 

Dave Smucker
Brasstown, NC

-----Original Message-----
From: theforge-bounces at mailman.qth.net [mailto:theforge-bounces at mailman.qth.net] On Behalf Of Ron Childers
Sent: Monday, August 14, 2017 10:42 AM
To: Blacksmithing List Sponsored by ABANA
Subject: Re: [TheForge] Old band saw blade

Thanks, L-6, even if it has carbide teeth brazed onto it? 

-----Original Message-----
From: theforge-bounces at mailman.qth.net [mailto:theforge-bounces at mailman.qth.net] On Behalf Of J. Petrila
Sent: Monday, August 14, 2017 10:37 AM
To: Blacksmithing List Sponsored by ABANA <theforge at mailman.qth.net>
Subject: Re: [TheForge] Old band saw blade

15n20 usually for high speed m42 blades. I believe wood mizer are 15n20 also.

L6 for circular.

You can test by seeing if a test strip will air harden..



On Aug 14, 2017 6:11 AM, "Ron Childers" <ron at munlaw.net> wrote:

I have a piece of old band saw blade without carbide teeth, probably from a Wood Miser. What kind of steel is it likely to be? 15N20 maybe? What steel is used in circular saw blade that has carbide teeth? Thanks, Ron ______________________________________________________________
TheForge mailing list
Home: http://mailman.qth.net/mailman/listinfo/theforge
Help: http://mailman.qth.net/mmfaq.htm
Post: mailto:TheForge at mailman.qth.net

TheForge mail list group photo site is
http://www.shutterfly.com
Login: blacksmithblacksmith at hotmail.com
Password: anvil

This list hosted by: http://www.qsl.net
Please help support this email list: http://www.qsl.net/donate.html Message delivered to jlpservicesinc at gmail.com ______________________________________________________________
TheForge mailing list
Home: http://mailman.qth.net/mailman/listinfo/theforge
Help: http://mailman.qth.net/mmfaq.htm
Post: mailto:TheForge at mailman.qth.net

TheForge mail list group photo site is
http://www.shutterfly.com
Login: blacksmithblacksmith at hotmail.com
Password: anvil

This list hosted by: http://www.qsl.net
Please help support this email list: http://www.qsl.net/donate.html Message delivered to ron at munlaw.net ______________________________________________________________
TheForge mailing list
Home: http://mailman.qth.net/mailman/listinfo/theforge
Help: http://mailman.qth.net/mmfaq.htm
Post: mailto:TheForge at mailman.qth.net

TheForge mail list group photo site is
http://www.shutterfly.com
Login: blacksmithblacksmith at hotmail.com
Password: anvil

This list hosted by: http://www.qsl.net
Please help support this email list: http://www.qsl.net/donate.html Message delivered to davesmucker at hotmail.com ______________________________________________________________
TheForge mailing list
Home: http://mailman.qth.net/mailman/listinfo/theforge
Help: http://mailman.qth.net/mmfaq.htm
Post: mailto:TheForge at mailman.qth.net

TheForge mail list group photo site is
http://www.shutterfly.com
Login: blacksmithblacksmith at hotmail.com
Password: anvil

This list hosted by: http://www.qsl.net
Please help support this email list: http://www.qsl.net/donate.html Message delivered to newenglandforge at aol.com

______________________________________________________________
TheForge mailing list
Home: http://mailman.qth.net/mailman/listinfo/theforge
Help: http://mailman.qth.net/mmfaq.htm
Post: mailto:TheForge at mailman.qth.net

TheForge mail list group photo site is
http://www.shutterfly.com
Login: blacksmithblacksmith at hotmail.com
Password: anvil

This list hosted by: http://www.qsl.net
Please help support this email list: http://www.qsl.net/donate.html Message delivered to davesmucker at hotmail.com


More information about the TheForge mailing list