I'm not familiar with D67A, how does it compare to other knife steels? L6 makes a good skinner and 5160 is good for a chopper....

 
-----Original Message-----
From: theforge-bounces at mailman.qth.net [mailto:theforge-bounces at mailman.qth.net] On Behalf Of Michael via TheForge
Sent: Monday, August 14, 2017 3:06 PM
To: theforge at mailman.qth.net
Subject: Re: [TheForge] Old band saw blade


the material used for blades that have carbide teeth eb welded to it is D6A.