I was always told riveting use light hammer fast to upset edge of material.
Use slower heavy hammer to forge or move the center of the material.
On Mar 1, 2015 11:47 PM, "jerry Frost" <akfrosty at mtaonline.net> wrote:
> I use a 16oz ball pein on large, over 5/16" iron rivets. Does a treadle
> hammer rivet set save a lot of time?
>
> Sorry Pete I couldn't help it. <snicker>
>
> Jer
> -----Original Message-----
> From: TheForge [mailto:theforge-bounces at mailman.qth.net] On Behalf Of
> Peter
> Fels & Phoebe Palmer
> Sent: Sunday, March 1, 2015 8:20 PM
> To: Blacksmithing List Sponsored by ABANA
> Subject: Re: [TheForge] Rivet question
>
> Thanks Jerry and Bob.
> Yeah, got impatient and used the treadle hammer to rough set it in.
>
> On Mar 1, 2015, at 8:20 PM, Bob Ehrenberger <eforge at centurytel.net> wrote:
>
> From: TheForge [mailto:theforge-bounces at mailman.qth.net] On Behalf Of
> Peter
> Fels & Phoebe Palmer
> Sent: Sunday, March 1, 2015 2:20 PM
> To: Blacksmithing List Sponsored by ABANA
> Subject: Re: [TheForge] Test
>
> OK.BS question:
> I was assembling one of my jointed bottle openers ( one that i had to take
> back apart and forge on some more to get the parts to work right), and
> after
> i'd set down and headed the 1/4" brass rivet, i had to spend 15 minutes
> wiggling it back and forth to free it up.
> Both holes were hot punched and the mating surfaces were hand forged so
> nothing was accurately aligned.
> What's the best, quickest way to keep the parts moving freely after the
> rivet is set down?
>
> -- Reply---
> The best thing is to prevent the rivet from getting too tight in the first
> place.
> If you put a piece of card stock between the parts before riveting you can
> remove it after riveting and there should be some clearance. Also when
> setting the rivet the lighter the hammer you use the easier it is to keep
> the upset at the very end.
>
> Bob Ehrenberger
> Shelbyville, MO
>
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.shutterfly.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
>
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.shutterfly.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
>
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.shutterfly.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
>
More information about the TheForge
mailing list