[TheForge] Heads-up: Universal (?) "Tongs"
Peter Fels & Phoebe Palmer
artgawk at thegrid.net
Sun Nov 30 00:12:42 EST 2014
They look real handy!
But one reason traditional tong design persists,
is because they are so quick to repair when they get beat up.
This looks like the tool you wish to hell you had,
about every 2 years.
On Nov 29, 2014, at 7:29 PM, Dave Smucker <davesmucker at hotmail.com> wrote:
Bruce, Those indeed look good. I have several vise grips with welded on "special jaws" and these would work better with your tong hand fatherr from the fire.
Dave
----------------------------------------
> Date: Sat, 29 Nov 2014 21:01:37 -0500
> From: freemab222 at gmail.com
> To: theforge at mailman.qth.net
> Subject: [TheForge] Heads-up: Universal (?) "Tongs"
>
> Harbor Freight has an interesting locking pliers with a long reach:
>
> http://www.harborfreight.com/15-inch-long-reach-locking-pliers-97609.html
>
> It even is more-or-less straight from handle to jaws, unlike traditional
> Vise Grips.
>
> I bought one and plan to test it for those occasions when you simply can't
> find a tongs that will hold the work tightly.
>
> I suspect I'll eventually arc-weld different jaws to this thing, as it's
> capacity is 1/2" or less and the object grasped by thies is not quite in
> line with the "reins". Adding to the jaws could correct both of these
> limitations.
>
> Harbor Freight also sell a couple long-reach needle-nose pliers that might
> prove useful as well:
> http://www.harborfreight.com/16-inch-long-reach-pliers-set-38598.html
>
> The jaws on these are too lightweight to leave in the fire for long, but
> the reins are fairly substantial. I don't think the box jaw is a good
> choice for a hot tool, so keeping that cool might be important.
>
> Bruce
> NJ
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.shutterfly.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
______________________________________________________________
TheForge mailing list
Home: http://mailman.qth.net/mailman/listinfo/theforge
Help: http://mailman.qth.net/mmfaq.htm
Post: mailto:TheForge at mailman.qth.net
TheForge mail list group photo site is
http://www.shutterfly.com
Login: blacksmithblacksmith at hotmail.com
Password: anvil
This list hosted by: http://www.qsl.net
Please help support this email list: http://www.qsl.net/donate.html
More information about the TheForge
mailing list