Bruce,  Those indeed look good.  I have several vise grips with welded on "special jaws" and these would work better with your tong hand fatherr from the fire.

Dave

----------------------------------------
> Date: Sat, 29 Nov 2014 21:01:37 -0500
> From: freemab222 at gmail.com
> To: theforge at mailman.qth.net
> Subject: [TheForge] Heads-up: Universal (?) "Tongs"
>
> Harbor Freight has an interesting locking pliers with a long reach:
>
> http://www.harborfreight.com/15-inch-long-reach-locking-pliers-97609.html
>
> It even is more-or-less straight from handle to jaws, unlike traditional
> Vise Grips.
>
> I bought one and plan to test it for those occasions when you simply can't
> find a tongs that will hold the work tightly.
>
> I suspect I'll eventually arc-weld different jaws to this thing, as it's
> capacity is 1/2" or less and the object grasped by thies is not quite in
> line with the "reins". Adding to the jaws could correct both of these
> limitations.
>
> Harbor Freight also sell a couple long-reach needle-nose pliers that might
> prove useful as well:
> http://www.harborfreight.com/16-inch-long-reach-pliers-set-38598.html
>
> The jaws on these are too lightweight to leave in the fire for long, but
> the reins are fairly substantial. I don't think the box jaw is a good
> choice for a hot tool, so keeping that cool might be important.
>
> Bruce
> NJ
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.shutterfly.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
 		 	   		  


More information about the TheForge mailing list