[TheForge] Sand blaster problem: hose blows off
Jerry Frost
akfrosty at mtaonline.net
Mon Jul 22 00:28:31 EDT 2013
Depending on how old the hose is it may not be competent enough to stay
on at pressure. Rubber loses volatiles over time, it's what causes the
weather checking of old tires. the volatiles are what keep rubber flexible
Just because you can get the hose to stay on at pressure does NOT mean
it's going to stay on or in one piece.
Jer
On 7/21/2013 8:07 PM, Peter Fels & Phoebe Palmer wrote:
> Make a stout , 2 part clamp that bolts together?
> Look and see what the commercial ones look like if you wanna get fancy.
> I've done it with split pipe sections,
> Welded on studs on all 4 corners on one side to fit
> the heavy washers welded on the other 1/2 pipe.
> Tightened down convincingly.
>
> On Jul 21, 2013, at 5:50 PM, Mike Spencer wrote:
>
>
> I have this nice little sand blaster, not what you'd want to clean up a
> ship but okay for smallish stuff -- maybe a 10 gal. pressure tank.
> Had it for a couple of years and never used it. Now I need it.
>
> Only the hose keeps blowing off. Very heavy hose, slides over
> ribbed nipples on hand set and feed valve, held with wire hose clamps.
> Blew off at both ends (gun and feed) at different times.
>
> Gummed it on with silicone sealant and reset the clamps. Came off
> again. Potentially dangerous. Not good.
>
> Is there some kind of standard hose connector for sandblasters?
> Anybody have suggestions? Finding parts will involve a 75 mi. trip to
> the hot and sticky city. I could use some suggestions as a starting
> point.
>
> I could, of course, try gluing the hose on with JB Weld or Gorilla
> glue but the hose should be removable facilitate clearing any blockage
> in the valve on the bottom of the tank. So a successful glue job
> would require excess disassembly or PITA destructive methods for
> removal when maintainance is required.
>
>
> - Mike
>