[TheForge] anvil question

Jerry Frost akfrosty at mtaonline.net
Wed Mar 14 18:04:33 EDT 2012


Uh, no 70xx and 60xx rods are not the same stuff, 70xx rods are low hydrogen 
finish rods where 60 series rods are fast freeze and root rods. Unless 
things changed even numbers are DC and odd numbers are AC, 6011 and 6013 are 
AC and 6010 is DC. I certainly can be wrong about this, it's been a couple 
decades since I took a class.

60/70/ac/dc doesn't much matter for slop welds but I don't trust slop for 
anything important.

Jer
----- Original Message ----- 
From: "Ron Childers" <ron at munlaw.net>
To: "Blacksmithing List Sponsored by ABANA" <theforge at mailman.qth.net>
Sent: Wednesday, March 14, 2012 11:06 AM
Subject: Re: [TheForge] anvil question


> Isn't 7018 a bit harder than 6010? 6011 is the same steel as 6010 and
> works better with an AC buzz box but there is 7018 made for AC. I just
> used about 30# of 7018 on a friend's tire hammer and it seems to work
> fine if run a bit hotter. The anvil is 2' of train boxcar axel welded to
> a 6"x12" block of steel (3 12"x 6"x 2" slabs welded together.
>
> -----Original Message-----
> From: theforge-bounces at mailman.qth.net
> [mailto:theforge-bounces at mailman.qth.net] On Behalf Of Jerry Frost
> Sent: Tuesday, March 13, 2012 5:27 PM
> To: Blacksmithing List Sponsored by ABANA
> Subject: Re: [TheForge] anvil question
>
> E-6010 would be a better choice than hardfacing rod. what makes
> hardfacing
> rod abrasion resistant is the tungsten in the matrix and does nothing
> for an
> anvil except make it really REALLY hard to grind to shape.
>
> Buildup or filler rod for use before hardfacing is a LOT better. It
> flows
> well and is far more deflection and impact resistant. Most can be
> hardened
> to around r55-60 which is good for forging and is easily ground to
> finished
> shape/contour.
>
> Hardfacing rod is limited to one pass two if you can hit the second
> while
> the first is still at or above orange heat. Multiple passes causes it to
>
> spall and it doesn't bond to itself particularly well. Any flex in the
> subsurface will result in hardfacing checking and eventually spalling.
>
> That's my experience with the stuff over 20 years rebuilding our drill
> steel
> and experimenting.
> Jer
> ----- Original Message ----- 
> From: "Allen Ortery" <bluestoneforge at gmail.com>
> To: <theforge at mailman.qth.net>
> Sent: Sunday, March 11, 2012 9:47 PM
> Subject: [TheForge] anvil question
>
>
>>I just got done cleaning the paint off of an anvil I picked up last
>> fall the markings on the side are
>>     Y 1889 Y
>>        700kg
>>           7
>> any one know where it was made?   Also I think I read somewhere that
>> 6010 welding rod was best to repair the small chips on the edges and
>> the square horn, is that right?
>> Thanks for the help
>>
>> --
>> Allen Ortery
>> bluestoneforge at gmail.com
>> 309-368-7967
>> ______________________________________________________________
>> TheForge mailing list
>> Home: http://mailman.qth.net/mailman/listinfo/theforge
>> Help: http://mailman.qth.net/mmfaq.htm
>> Post: mailto:TheForge at mailman.qth.net
>>
>> TheForge mail list group photo site is
>> http://www.photoworks.com
>> Login: blacksmithblacksmith at hotmail.com
>> Password: anvil
>>
>> This list hosted by: http://www.qsl.net
>> Please help support this email list: http://www.qsl.net/donate.html
>>
>>
>> -----
>> No virus found in this message.
>> Checked by AVG - www.avg.com
>> Version: 2012.0.1913 / Virus Database: 2114/4866 - Release Date:
> 03/12/12
>>
>
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.photoworks.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.photoworks.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
>
>
> -----
> No virus found in this message.
> Checked by AVG - www.avg.com
> Version: 2012.0.1913 / Virus Database: 2114/4870 - Release Date: 03/14/12
> 



More information about the TheForge mailing list