[TheForge] Anvil Repair - 7018 Rod use
Vincent_Nakovics at nps.gov
Vincent_Nakovics at nps.gov
Wed Mar 14 12:41:53 EDT 2012
Thanks for the input Jerry,
I was worried that I had it wrong. We have repaired 2 anvils using the
preheat and 7018 method now. Last night was the first time I used my anvil
that I repaired just last week. after I was done making my piece I couldn
not resist tapping the edges that we repaired with my 3lb hammer. They
weren't full smashing blows, but you wouldn't want your fingers there. The
repair spots did not dent. I was happily impressed! The NJBA I believe did
a bunch of repairs and that's where I got all my info from. (I could be
wrong about the org, I just jotted down the pertinent stuff a while back.).
So far it has worked for the two that we have done. Preheat anvil, use 7018
Rod. grind, sand, walla!
Vince
More information about the TheForge
mailing list