[TheForge] Kinyon style hammer help
Kim George
klgeorge at kent.edu
Wed Oct 19 11:39:47 EDT 2011
Also check the trip valve.They have a tendency to get loose so that it
doesn't trip or delays tripping. also check the exhaust if your not
getting full flow there it will slow ram speed.
On 10/19/11, David E. Smucker <davesmucker at hotmail.com> wrote:
> Todd, A guess -- something is getting hot and getting tight. Could it be
> your ram guides? Could be your air cyclinder? Could it be you main spool
> valve? What feels hot to the touch?
>
> Dave Smucker
>
> -----Original Message-----
> From: Todd Rich
> Sent: Wednesday, October 19, 2011 9:43 AM
> To: Blacksmithing List Sponsored by ABANA
> Subject: [TheForge] Kinyon style hammer help
>
>
> Several years ago, I built a power hammer based off of the Kinyon plans.
> I did the modification with the regulator to balance strike and return
> pressures.
>
> Anyway, it seems to have a bit of a problem. After running for about 15
> minutes, the speed of the ram slows way down. This doesn't seem to have
> anything to do with the switch sticking (I installed a line oiler right
> before the sensor switch), or the height of the work. It seems to be
> mostly time of use related. I need some help in figuring out what is
> wrong and fixing it. I'm willing to post pictures or run tests as
> needed.
>
> Here is a link to a video I made shortly after I built it.
>
> http://www.youtube.com/watch?v=KkUFgoU_LO0
>
> Todd Rich
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.photoworks.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
>
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.photoworks.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
>
--
Kim George
"Why for you try to bury me in cold,cold ground?"
Taz
More information about the TheForge
mailing list