[TheForge] Anvil for a newbie

peter fels artgawk at thegrid.net
Tue May 10 12:20:14 EDT 2011


Go to a scrap yard  or a heavy equip repair place.....and get any elongate piece of steel with a large cross section and an end you can grind flat.
Heavy equipment axles, shafts, etc.

On May 10, 2011, at 4:02 AM, David C Kuhlman wrote:

> Unfortunately, none of those things seem to work in Vegas. Right now it's
> even hard to come by RR track or fork lift forks. One guy was trying to sell
> tines for $300 or more per pair.
> 
> -----Original Message-----
> From: theforge-bounces at mailman.qth.net
> [mailto:theforge-bounces at mailman.qth.net] On Behalf Of peter fels
> Sent: Monday, May 09, 2011 7:05 PM
> To: Blacksmithing List Sponsored by ABANA
> Subject: Re: [TheForge] Anvil for a newbie
> 
> Matt;
> Contrary to popular opinion, RR track makes a lousy anvil.
> The extra heavy RR track used in HD switches is a bit better.
> Using either heavy Track or the heaviest shaft you can snag...
> Plant it upright in the ground and forge on the butt end.
> That way you have the mass directly under the hammer
> where it needs to be, for effective forging.
> A lot of horizontal mass , like in RR track anvils, is good for jewelry
> forging.
> Go to your local BS group's meets and check the tailgate sales...talk to old
> rural folks,
> put an ad in the local cheap classifieds and craigs' list. There are anvils
> around, unclaimed..
> You just have to out-sleuth all the other anvil seekers.
> It generally takes some persistence to find yr anvil...
> but then, it sure helps to be stubborn in this medium.
> 
> 
> TheForge mail list group photo site is
> http://www.photoworks.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
> 
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
> 
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
> 
> TheForge mail list group photo site is
> http://www.photoworks.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
> 
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html



More information about the TheForge mailing list