[TheForge] Home-made grinders and wire brushes

Bob Ehrenberger eforge at centurytel.net
Thu Jun 23 16:21:30 EDT 2011


No, They look like a wire wheel, but instead of wire it is made up with a 
bunch of small (16 ga) stiff rods that are made of nylon or some other 
plastic/composit material. They look like and work like a wire wheel just 
not quite as agressive and the rods ware down instead of breaking off.

Robert Ehrenberger
Shelbyville, Mo.
eforge at centurytel.net


----- Original Message ----- 
From: <blakkpawss at yahoo.com>
To: "Bob Ehrenberger" <eforge at centurytel.net>; "Blacksmithing List Sponsored 
by ABANA" <theforge at mailman.qth.net>
Sent: Thursday, June 23, 2011 12:44 PM
Subject: Re: [TheForge] Home-made grinders and wire brushes


So, they are something like the Scotchbrite wheels or the 3M paint stripping 
wheels then I would guess?
Sent from my BlackBerry® smartphone powered by Alltel

-----Original Message-----
From: "Bob Ehrenberger" <eforge at centurytel.net>
Sender: theforge-bounces at mailman.qth.net
Date: Thu, 23 Jun 2011 12:39:28
To: theforge<theforge at mailman.qth.net>
Reply-To: Bob Ehrenberger <eforge at centurytel.net>,
Blacksmithing List Sponsored by ABANA <theforge at mailman.qth.net>
Subject: Re: [TheForge] Home-made grinders and wire brushes

A few years ago I got a deal on a bunch of wire wheels that were made of
some kind of nylon/fiber. They are not as agressive as steel wire wheels,
but they never break off. They just gradually ware down until they are gone.
One problem, they melt so can't be used on hot steel.

Robert Ehrenberger
Shelbyville, Mo.
eforge at centurytel.net


______________________________________________________________
TheForge mailing list
Home: http://mailman.qth.net/mailman/listinfo/theforge
Help: http://mailman.qth.net/mmfaq.htm
Post: mailto:TheForge at mailman.qth.net

TheForge mail list group photo site is
http://www.photoworks.com
Login: blacksmithblacksmith at hotmail.com
Password: anvil

This list hosted by: http://www.qsl.net
Please help support this email list: http://www.qsl.net/donate.html



-----
No virus found in this message.
Checked by AVG - www.avg.com
Version: 10.0.1382 / Virus Database: 1513/3721 - Release Date: 06/23/11



More information about the TheForge mailing list