[TheForge] Home-made grinders and wire brushes

peter fels artgawk at thegrid.net
Thu Jun 23 19:24:11 EDT 2011


The plastic rods or fibers have a graded abrasive embedded in the plastic .
They will not aggressively rip everything off a surface like a stiff wire brush...
on the other hand, neither will they instantly remove all the meat from your knuckles.

On Jun 23, 2011, at 1:21 PM, Bob Ehrenberger wrote:

> No, They look like a wire wheel, but instead of wire it is made up with a 
> bunch of small (16 ga) stiff rods that are made of nylon or some other 
> plastic/composit material. They look like and work like a wire wheel just 
> not quite as agressive and the rods ware down instead of breaking off.
> 
> Robert Ehrenberger
> Shelbyville, Mo.
> eforge at centurytel.net
> 
> 
> ----- Original Message ----- 
> From: <blakkpawss at yahoo.com>
> To: "Bob Ehrenberger" <eforge at centurytel.net>; "Blacksmithing List Sponsored 
> by ABANA" <theforge at mailman.qth.net>
> Sent: Thursday, June 23, 2011 12:44 PM
> Subject: Re: [TheForge] Home-made grinders and wire brushes
> 
> 
> So, they are something like the Scotchbrite wheels or the 3M paint stripping 
> wheels then I would guess?
> Sent from my BlackBerry® smartphone powered by Alltel
> 
> -----Original Message-----
> From: "Bob Ehrenberger" <eforge at centurytel.net>
> Sender: theforge-bounces at mailman.qth.net
> Date: Thu, 23 Jun 2011 12:39:28
> To: theforge<theforge at mailman.qth.net>
> Reply-To: Bob Ehrenberger <eforge at centurytel.net>,
> Blacksmithing List Sponsored by ABANA <theforge at mailman.qth.net>
> Subject: Re: [TheForge] Home-made grinders and wire brushes
> 
> A few years ago I got a deal on a bunch of wire wheels that were made of
> some kind of nylon/fiber. They are not as agressive as steel wire wheels,
> but they never break off. They just gradually ware down until they are gone.
> One problem, they melt so can't be used on hot steel.
> 
> Robert Ehrenberger
> Shelbyville, Mo.
> eforge at centurytel.net
> 
> 
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
> 
> TheForge mail list group photo site is
> http://www.photoworks.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
> 
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
> 
> 
> 
> -----
> No virus found in this message.
> Checked by AVG - www.avg.com
> Version: 10.0.1382 / Virus Database: 1513/3721 - Release Date: 06/23/11
> 
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
> 
> TheForge mail list group photo site is
> http://www.photoworks.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
> 
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html



More information about the TheForge mailing list