Hi Karen:
Sand blasters are neat! You can literally carve steel, glass or stone 
with them.
The rough surface has a lot of extra surface area leaving it very 
vulnerable to rust.
Different blast media produce different finishes.
Wax works..any sealant almost, will work for a while....indoors. Keep 
reapplying it for maintenance.
And you can get much fancier from there
Fingerprints, oil, dust from the blasting get in the way.
We recently had a related discussion.

On 11/4/2010 11:23 AM, ~K~ wrote:
> Hey other metal folks!
>
> I just got overly excited about a sand blaster I had access to for an afternoon. I took the scale off a little steel piece I made. Forgot how porous it makes the steel. Is there a coating I can put on the will stop the finger marks but maintain at least a bit of the finish? Wax maybe?
>
> ~Karen~
> Sent on the TELUS Mobility network with BlackBerry
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.photoworks.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
>


More information about the TheForge mailing list