what about washing it with Phospho right away, would that help?
I'm not really sure what the phosphoric acid preps actually DO on clean
metal, obviously they neutralize oxides, but do they stabilize steel
surfaces that DON'T have oxides on them?
Andy G.
-----Original Message-----
From: peter fels & phoebe palmer
Sent: Friday, November 05, 2010 1:49 AM
To: lucky7steel at gmail.com ; Blacksmithing List Sponsored by ABANA
Subject: Re: [TheForge] post sand blasting
Hi Karen:
Sand blasters are neat! You can literally carve steel, glass or stone
with them.
The rough surface has a lot of extra surface area leaving it very
vulnerable to rust.
Different blast media produce different finishes.
Wax works..any sealant almost, will work for a while....indoors. Keep
reapplying it for maintenance.
And you can get much fancier from there
Fingerprints, oil, dust from the blasting get in the way.
We recently had a related discussion.
On 11/4/2010 11:23 AM, ~K~ wrote:
> Hey other metal folks!
>
> I just got overly excited about a sand blaster I had access to for an
> afternoon. I took the scale off a little steel piece I made. Forgot how
> porous it makes the steel. Is there a coating I can put on the will stop
> the finger marks but maintain at least a bit of the finish? Wax maybe?
>
> ~Karen~
> Sent on the TELUS Mobility network with BlackBerry
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.photoworks.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
>
______________________________________________________________
TheForge mailing list
Home: http://mailman.qth.net/mailman/listinfo/theforge
Help: http://mailman.qth.net/mmfaq.htm
Post: mailto:TheForge at mailman.qth.net
TheForge mail list group photo site is
http://www.photoworks.com
Login: blacksmithblacksmith at hotmail.com
Password: anvil
This list hosted by: http://www.qsl.net
Please help support this email list: http://www.qsl.net/donate.html
More information about the TheForge
mailing list