[TheForge] metalworking question- soldering brass
Woolley
wjec1 at verizon.net
Wed Jan 20 18:17:02 EST 2010
Sounds like a pita job but I can relate. I have never been asked to do
such a thing and would definitely prefer tig myself. I would love to
see pictures of this project and or weld joint.
Andy Gladish wrote:
> Thanks so much, this is exactly the info I need.
> Any recommendations for a suitable solder?
> Also, what about preparation? Using jewelry solder, I've always cleaned
> with an acid bath- would filing and flux be suitable?
> It's not so much perfect preservation of the patina, more that we don't
> want to get into having to polish the entire length because of a joint
> needing to be filed/sanded smooth.
> Originally, they liked my TIG/silicon bronze welds, but then it seems a
> finer joint was needed- I'm still lobbying for TIG and some minimal
> smoothing, but we'll see...
> Andy
>
> On Wed, 20 Jan 2010 12:47:43 -0800, Bruce Freeman <freemab222 at gmail.com>
> wrote:
>
>
>> non-eutectic solder
>>
>
>
>
More information about the TheForge