[TheForge] metalworking question- soldering brass
Andy Gladish
gladish at cablerocket.com
Wed Jan 20 18:31:48 EST 2010
The railing project is on my work blog, ElementFe.Blogspot.com but we
haven't begun installing the handrail, just experimenting at home with
different joint treatments for now.
Sometimes PITA can mean, "Pays very well If you can handle The chAllenge"
(not very good, I know...blame it on welding fumes)(Different from an
organization I belong to, PETA- People Eating Tasty Animals)
Andy G.
On Wed, 20 Jan 2010 15:17:02 -0800, Woolley <wjec1 at verizon.net> wrote:
> Sounds like a pita job but I can relate. I have never been asked to do
> such a thing and would definitely prefer tig myself. I would love to
> see pictures of this project and or weld joint.