[TheForge] Re: Induction Forges (was Re: Slack tank...POL OT)
Mike Spencer
mspencer at tallships.ca
Wed Dec 22 15:15:10 EST 2010
> I was at a hammer-in last weekend and used one. Wow! I gots to get
> me one of these!
>
> http://superiorinduction.thomasnet-navigator.com/viewitems/induction-heaters/mf-series-induction-heaters?
>
> I was actually using it to do some small forge welds. It took cold
> 7/16" stock up to welding heat in about 15 seconds. The heat is very
> localized.
We've come a long way from Lumpkin, Georgia, haven't we?
--