[TheForge] Induction Forges (was Re: Slack tank...POL OT)
Paul N
crosspein at sbcglobal.net
Wed Dec 22 14:03:52 EST 2010
I was at a hammer-in last weekend and used one. Wow! I gots to get me
one of these!
http://superiorinduction.thomasnet-navigator.com/viewitems/induction-heaters/mf-series-induction-heaters?
I was actually using it to do some small forge welds. It took cold 7/16"
stock up to welding heat in about 15 seconds. The heat is very localized.
You can make your own coils to whatever size and shape you want.
They cost about $3k, but I want one.
**paul
On 12/22/10 12:36 PM, Andrew Vida wrote:
>
>
...
> Speaking of energy sources, does anyone here use induction coils? For
> some apps they appear ideal. I am wondering if they can be arranged
> such that there is open space along the coil wall to accommodate odd
> shapes. Anyone?
>>
>>
>