[TheForge] Fw: Anvil repair

peter fels & phoebe palmer artgawk at thegrid.net
Sun Dec 12 13:53:24 EST 2010



On 12/12/2010 6:58 AM, Andrew Vida wrote:
> Just had a thought, so take cover.
>
> Has anyone ever tried welding a face using thermit?  A think layer of
> thermit interposed between the wrought body and steel face, clamped
> elastically perhaps?  Light bugger off and watch the fun!
Maybe with a scarfed face bottom in a hydr press with refractory dams 
around the edges of the weld?
The steel i saw flow in a thermite demo was really  a pretty low 
viscosity liquid.
I think the Fisher anvils were poured over a tool steel face.
Seeing as they forge welded the major elements of the wrought anvils 
together,
the tool steel face wouldn't have seemed such a leap.
>
>
> CGRAF wrote:
>> I seem to remember ( and Seeming to remember is happening more and more)
>> that some of the tool steel tops were welded to the base of cast anvils
>> by placing the heated steel plate in the mold and pouring the cast over it.
>>
>> It might work, but I cannot find any corroborating documents in my piles
>> of crap.
>>
>> At any rate it sounds less nasty than trying to forge weld a 3/4 inch
>> plate onto a base.
>>
>> Am I remembering something real or just a dream?
>>
>> Mike Graf
>> ______________________________________________________________
>> TheForge mailing list
>> Home: http://mailman.qth.net/mailman/listinfo/theforge
>> Help: http://mailman.qth.net/mmfaq.htm
>> Post: mailto:TheForge at mailman.qth.net
>>
>> TheForge mail list group photo site is
>> http://www.photoaccess.com
>> Login: blacksmithblacksmith at hotmail.com
>> Password: anvil
>>
>> This list hosted by: http://www.qsl.net
>> Please help support this email list: http://www.qsl.net/donate.html
>>
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.photoworks.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
>


More information about the TheForge mailing list