Figure out what your offset is and drill from each side then hand drill
between the holes to get the angles like a reamer. Make a easy drill guide,
hole with pin or rivet and where you want the next hole. If you have a lot
of holes to drill, make several of the guides at the beginning of the job
not from each other after they are worn.
L Brown