Very interesting approach, since the toughest thing I need to drill is
some 1/2" flat bar, that technique might work really well, and would be
sort of self correcting for the angle-thanks!
On Fri, 13 Mar 2009 02:08:12 -0700, Larry Brown <lp.brown at verizon.net>
wrote:
>
> Figure out what your offset is and drill from each side then hand drill
> between the holes to get the angles like a reamer. Make a easy drill
> guide,
> hole with pin or rivet and where you want the next hole. If you have a
> lot
> of holes to drill, make several of the guides at the beginning of the job
> not from each other after they are worn.