[TheForge] drilling question

Woolley wjec1 at verizon.net
Wed Mar 11 09:17:36 EDT 2009


Andy Gladish wrote:
> Thanks Ries and Andy, lots to go on there.
> It's a little off topic cause there's not a forged scrap in this railing,  
> and I don't get to choose whether it's drilled or not...
> I'll try the jig if just drilling and reaming won't do it. Fortunately,  
> the holes go in square tube rather than solid, so it's easier to abuse  
> that way.
> Andy G.
>
>   

I did a railing that round 3/8 "or 1/2" stock passed through 1 1/4" 
square tubing at an angle.  I drilled then shaped with a straight 
grinder with deburring bits.. Lot of work.