Roger Degner wrote:
> If you can dip your copper go to Wal-Mart and buy a jug of PH minus powder.
> Mix with warm water. 10# should do 50 gal or so of solution.
> Use a plastic container
> Makes copper a bright pink some scotch bright pad scrubbing may be
> necessary.
> It is sodium bisulphate which I think is the same as sparex but a lot
> cheaper.
>
> Roger R Degner
Another source for the sodium bisulphate is Iron Out, used to clean iron
stains on clothing and to remove iron contamination from your water softener
--
Paul Sperbeck WB9HCO
"The difference between genius and stupidity is that
genius has its limits." -Albert Einstein
"Life is hard...it's harder if you're stupid" John Wayne - Sands of Iwo Jima
"We started off trying to set up a small anarchist community, but people
wouldn't obey the rules." -- Alan Bennett
No trees were killed in the sending of this message, but a large number
of electrons
were terribly inconvenienced.
More information about the TheForge
mailing list