In the shop where I work we have made a copper coil (5/8") 19"
diameter, 24" tall.
Silver soldered the coil to 1/8' copper legs. Used propane / oxy for heat.
Now I need to clean the flux and discoloration from the assembly.
Looking for info on the best way to clean it.
thanks,
dave mudge
______________________________________________________________
TheForge mailing list
Home: http://mailman.qth.net/mailman/listinfo/theforge
Help: http://mailman.qth.net/mmfaq.htm
Post: mailto:TheForge at mailman.qth.net
TheForge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
Password: anvil
This list hosted by: http://www.qsl.net
Please help support this email list: http://www.qsl.net/donate.html
More information about the TheForge
mailing list