Care to share any information and suppliers on this process?
Never saw it done, have used the stuff  done by others alot
Larry Brown

>We use ALOT of wire rope and bridge strand for any given project and make 
>our own connections using spelter (hot zinc) socketing. We do this quite a 
>bit in the field and it's easier than most people think. It's also much 
>stronger and secure than cable clips or swaged fittings.
>
>
>Steve
>