[TheForge] low carbon sheet
Bruce Freeman
freemab222 at gmail.com
Sun Sep 14 16:00:02 EDT 2008
On second thought, FIRST find out whether the "enamel" is just paint.
Soak it in strong alkali - caustic soda or washing soda. Paint will
be gone pretty quickly in these, with no harm to the metal.
On Sun, Sep 14, 2008 at 3:58 PM, Bruce Freeman <freemab222 at gmail.com> wrote:
> Think of the enamel as flux...
>
> On Sun, Sep 14, 2008 at 11:05 AM, Andrew Vida <osan at netlabs.net> wrote:
>> Deep draw sheet should be called AXDQ, IIRC. There are also newer,
>> supposedly superior steels as well.
>>
>> A good place to find deep draw sheet is the scrap yard or the curb. Washers,
>> dryers, refrigerators, freezers, and stoves (non-stainless) are all made
>> from it. That is, their outer structures. the one problem may be getting
>> the enamel off.
>
> --
> Bruce
> NJ
>
--
Bruce
NJ
More information about the TheForge