[TheForge] low carbon sheet
Bruce Freeman
freemab222 at gmail.com
Sun Sep 14 15:58:09 EDT 2008
Think of the enamel as flux...
On Sun, Sep 14, 2008 at 11:05 AM, Andrew Vida <osan at netlabs.net> wrote:
> Deep draw sheet should be called AXDQ, IIRC. There are also newer,
> supposedly superior steels as well.
>
> A good place to find deep draw sheet is the scrap yard or the curb. Washers,
> dryers, refrigerators, freezers, and stoves (non-stainless) are all made
> from it. That is, their outer structures. the one problem may be getting
> the enamel off.
--
Bruce