I could be wrong, but I don't think that you want to anneal the metal in 
a bell.  It will certainly alter the tonal characteristic, and I am 
fairly sure that it will dull it.

Peter Hirst wrote:
> Annealing brass:  dull red & water
> quench.
> 
> 
> ----- Original Message ----- From: "Franklin Police" <780 at mchsi.com>
> To: <munlaw2 at hcsmail.com>; "'Blacksmithing List Sponsored by ABANA'" 
> <theforge at mailman.qth.net>
> Sent: Thursday, October 02, 2008 5:48 PM
> Subject: RE: [TheForge] RE: Tarnished brass
> 
> 
> Not sure about brass but to clean copper we use HTH brand PH minus from
> Walmart.
> Mix the powder with hot water and let soak in plastic bucket.
> 
> Did you anneal while making the bell
> I bought a few shells and was thinking about doing some trench art with 
> them
> like I do copper pipe.  Anyone have suggestions on annealing?
> 
> Roger R Degner
> 
> 
> 
> 
> What is the quickest way to clean tarnish off a brass 90mm cannon shell? I
> made a bell out of it and would like to shine it up, but Brasso hardly
> touched it.
> 
> Ron C
> 
> 
> 
> 
> 
> 
> 
> 
> 
> **************************************************************************** 
> 
> ********
> This footnote confirms that this email message has been scanned by PineApp
> Mail-SeCure for the presence of malicious code, vandals & computer viruses.
> **************************************************************************** 
> 
> ********
> 
> 
> 
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is http://www.photoaccess.com
> Login:  blacksmithblacksmith at hotmail.com
> password:  anvil
> ___________
> 
> 
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  blacksmithblacksmith at hotmail.com
> password:  anvil
> ___________
> 
> 
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  blacksmithblacksmith at hotmail.com
> password:  anvil
> ___________
> 
> 

-- 

	-Andy V.

You made them strong.
We make them Army dead.


More information about the TheForge mailing list