> From: "Rich Maynard" <rich at maynard.org.uk>
> Subject: RE: [TheForge] Punching and drifting angled holes
> To: "'Blacksmithing List Sponsored by ABANA'"
> <theforge at mailman.qth.net>
> Message-ID: <001c01c8b9d3$4f8e1a10$0201a8c0 at TC1100>
> Content-Type: text/plain; charset="US-ASCII"
>
> I've never tried it and I'm working from home today but I'd try
> punching
> them straight then re-heating and twisting to the right angle with a
> cold
> bar. It's not going to be a nice clean hole so might not be
> appropriate but
> the final shape will witness the process that created it which is
> one of the
> things I love about forged stuff.
>
> Rich M.
>
> Richard Maynard - Artist Blacksmith
> The Forge, Much Hadham, Hertfordshire SG10 6BS
>
> The Forge Experience - be a blacksmith for a day!
> http://www.muchhadhamforge.co.uk/experience.pdf
>
> rich at muchhadhamforge.co.uk
> www.muchhadhamforge.co.uk
More information about the TheForge
mailing list