Wow.....deja-vu...like working for the federal govt all over again!
Don't forget to first undersize round drift first, THEN final drift, THEN
block. Otherwise, the pooch will bite back
Woof
Grant
-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net]On Behalf Of Rick Korinek
Sent: Thursday, May 22, 2008 7:48 PM
To: 'Blacksmithing List Sponsored by ABANA'
Subject: RE: [TheForge] Re: Punching and drifting angled holes
Grant,
Your description of slitting on an angle was very good. It's just that no
good deed should go unpunished.
-Rick
-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net] On Behalf Of Grant Marcoux
Sent: Wednesday, May 21, 2008 2:36 PM
To: Blacksmithing List Sponsored by ABANA
Subject: RE: [TheForge] Re: Punching and drifting angled holes
Woof-Woof.....Snort.....Moo...Oink I'm having an animal crisis Grant
-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net]On Behalf Of Jerry Frost
Sent: Tuesday, May 20, 2008 11:50 AM
To: Blacksmithing List Sponsored by ABANA
Subject: Re: [TheForge] Re: Punching and drifting angled holes
I CAN'T believe I missed a straight line like THAT!
I am SOOO slipping in my old age!
Frosty
-------------------------------
If it ain't forged
it ain't real.
Wrought iron is.
The FrostWorks
Meadow Lakes, AK.
From: "Rick Korinek" <rickkorinek at verizon.net>
> "Do not hit the pooch directly with the hammer."
> -Grant
>
> Grant, I did not know you were also a dog whisperer.
>
> -Rick
>
>
>
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
password: anvil
___________
No virus found in this incoming message.
Checked by AVG.
Version: 7.5.524 / Virus Database: 269.23.21/1456 - Release Date: 5/20/2008
6:45 AM
No virus found in this outgoing message.
Checked by AVG.
Version: 7.5.524 / Virus Database: 269.23.21/1458 - Release Date: 5/21/2008
7:21 AM
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
password: anvil
___________
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
password: anvil
___________
No virus found in this incoming message.
Checked by AVG.
Version: 7.5.524 / Virus Database: 269.24.0/1460 - Release Date: 5/22/2008
7:06 AM
No virus found in this outgoing message.
Checked by AVG.
Version: 7.5.524 / Virus Database: 269.24.0/1460 - Release Date: 5/22/2008
7:06 AM
More information about the TheForge
mailing list