[TheForge] Band saw blades
robert hensarling
rhrocker at hilconet.com
Fri Mar 7 12:38:02 EST 2008
You mentioned that the neat thing is welding etc. I have a 20" Delta and
one the face of it is a small grinding wheel, then after you grind a taper
on both ends, you clamp the blade where you want to weld, then touch a
button and it welds. The grinder is then used again to clean up the weld
(no thump, thump,thump, etc). This is the good thing!!! The bad thing is
that I can't get it to work (the arc weld feature). Also there's no info
about flux, etc.
I guess the clamping fixture could also be used to hold the ends securely
while I silver soldered and ground.
Can any one hazard a guess as to why the arc welder won't work? I don't
think it's fused, I think it picks up it's juice from the input box hanging
on the side. Could be fused between that box and the arc welder eh?
Ok, Whoa! I really got off the well beaten path. Apologies, and back to
you guys.
----- Original Message -----
From: "Ron Childers" <munlaw2 at hcsmail.com>
To: "'Sponsored by ABANA'" <theforge at mailman.qth.net>
Sent: Friday, March 07, 2008 6:44 AM
Subject: RE: [TheForge] Band saw blades
Holly is local; we used to have a half dozen industrial supply places here,
any one of which could make up blades. The neat setup is an electric spot
welder made for the purpose of welding band saw blades.
Ron C
-----Original Message-----
From: theforge-bounces at mailman.qth.net
[mailto:theforge-bounces at mailman.qth.net] On Behalf Of PlumDon at aol.com
Sent: Thursday, March 06, 2008 4:55 PM
To: theforge at mailman.qth.net
Subject: Re: [TheForge] Band saw blades
In a message dated 3/6/2008 7:38:22 AM Eastern Standard Time,
mobjak at yahoo.com writes:
Did you check Enco? They are typically less expensive
(of course most companies are) than McMaster Carr.
Thanks for the info re bandsaw blades,folks. Enco did not have the size and
no Holly, Inc nearby. But I did find a source a bit cheaper than McMaster
and
the same size, etc., that Jim recommended: Sunbelt Industrial
A while ago there was some discussion on glass doors for fireplace screens.
I think even some notes about how to and technique. Did anyone, perchance,
keep those notes and could pass them back to me.
Kindest thanks
Don Plummer
**************It's Tax Time! Get tips, forms, and advice on AOL Money &
Finance. (http://money.aol.com/tax?NCID=aolprf00030000000001)
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
password: anvil
___________
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: blacksmithblacksmith at hotmail.com
password: anvil
___________
More information about the TheForge
mailing list