I use a half and half mixture of boric acid and black iron oxide. Both of these items I get from Standard Ceramic Supply in Pittsburgh, PA. It works very well and only a little more costly than 20 mule team. Jonathan Nedbor gave me the recipe.
Mark Williams
Snow Hill, Maryland
-------------- Original message --------------
From: "David E. Smucker" <davesmucker at hotmail.com>
> Some smiths around here use a flux that is a mixture of boric acid (roach
> kill) and iron oxide. They get the iron oxide from the pottery suppliers.
> I don't understand the chemistry of what is happening at the melt
> temperatures. This flux seems to work very well for them.
>
> Dave
> ----- Original Message -----
> From: "Peter Hirst"
> To: ; "Sponsored by ABANA"
> Sent: Monday, April 14, 2008 10:37 PM
> Subject: Re: [TheForge] Re: New Discoveries: Ersatz EZ Weld
>
>
> > Except band saw bits are steel. Grinder bits are oxide. I'm not sure
> > what good they do in flux. In fact, i am wondering if the spec sheet I
> > saw on EZ weld could be correct. Silica slag, sure. But oxides?
> >
> >
> >
> > ----- Original Message -----
> > From: "Mike Spencer"
> > To:
> > Sent: Monday, April 14, 2008 10:10 PM
> > Subject: [TheForge] Re: New Discoveries: Ersatz EZ Weld
> >
> >
> >>
> >>> So do I throw a bunch of scale or grinder dust in with the borax an
> >>> steel shavings?
> >>
> >> If you collect the grinder dust (or band saw chips) with a magnet, you
> >> can (mostly) exclude non-ferrous bits, glass- and abrasive-dust
> >> from the wheel, underbody roadgrime and other unwanted detritus.
> >>
> >> Or maybe that doesn't matter.
> >>
> >>
> >> - Mike
> >>
> >> --
> >> Michael Spencer Nova Scotia, Canada .~.
> >> /V\
> >> mspencer at tallships.ca /( )\
> >> http://home.tallships.ca/mspencer/ ^^-^^
> >> _______________________________________________
> >> Manage membership or unsubscribe at:
> >> http://mailman.qth.net/mailman/listinfo/theforge
> >> theforge mail list group photo site is
> >> http://www.photoaccess.com
> >> Login: blacksmithblacksmith at hotmail.com
> >> password: anvil
> >> ___________
> >>
> >>
> >>
> >
> > _______________________________________________
> > Manage membership or unsubscribe at:
> > http://mailman.qth.net/mailman/listinfo/theforge
> > theforge mail list group photo site is
> > http://www.photoaccess.com
> > Login: blacksmithblacksmith at hotmail.com
> > password: anvil
> > ___________
> >
> >
> >
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
More information about the TheForge
mailing list