[TheForge] brass
Wayne Ackman
stryker at vulcanproductions.us
Sat Oct 20 16:26:51 EDT 2007
Thanks Dan.
I thought I needed some very fine sandpaper, didn't know it was
available at the auto parts store. Ran down and got some and this
works. Appreciate the help
Wayne
Dan Scheid wrote:
> If you don't mine hand work then use sandpaper. Start with 150 grit and go
> to 1500 then hit it with a polisher. You can get up to 1500 wet sanding
> paper at an auto supplier in the paint department. If you want the quick
> dirty way use a dremal tool with SS buffing compound
> Dan Scheid
>
.