If you don't mine hand work then use sandpaper. Start with 150 grit and go
to 1500 then hit it with a polisher. You can get up to 1500 wet sanding
paper at an auto supplier in the paint department. If you want the quick
dirty way use a dremal tool with SS buffing compound
Dan Scheid
Morning all;

I have a small job requiring brass pieces 3 foot long bent 90 degrees 
along the length.  the bender left marks on the surface.  I have been 
experimenting on how best to get a clean shiny surface.  I don't believe 
I have the proper abrasives to get this done.  I am trying to remove all 
the scratches.  It looks like I need to order something to get this done 
right.  So I am asking the brain trust, what will work, and where do you 
suggest I order it.  There isn't much around here, so I will probably 
have to order online. 

Wayne
_______________________________________________
Manage membership or unsubscribe at:
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login:  blacksmithblacksmith at hotmail.com
password:  anvil
___________


No virus found in this incoming message.
Checked by AVG Free Edition. 
Version: 7.5.488 / Virus Database: 269.15.3/1081 - Release Date: 10/19/2007
5:41 PM
 

No virus found in this outgoing message.
Checked by AVG Free Edition. 
Version: 7.5.488 / Virus Database: 269.15.3/1081 - Release Date: 10/19/2007
5:41 PM
 



More information about the TheForge mailing list