[TheForge] new question, quenching oil
Lon Humphrey
ironcrossforge at roadrunner.com
Mon Nov 12 14:04:13 EST 2007
i use hydro oil mixed with desil fuel to thin it out a bit....im working
52100 with good results.....over 200 cuts on sisal rope b4 it goes dull
----- Original Message -----
From: "David E. Smucker" <davesmucker at hotmail.com>
To: "Sponsored by ABANA" <theforge at mailman.qth.net>
Sent: Monday, November 12, 2007 1:08 PM
Subject: Re: [TheForge] new question, quenching oil
> The primary oil I use for oil quenching is used hydraulic oil. Hydraulic
> oil today is generally straight mineral oil with R & O additives. (R & O,
> is Rust and Oxidation). It has worked very well for me. I thin it a bit
> by adding diesel oil but other wise use it straight from a hydraulic oil
> change on the tractor. It DOES NOT smell near as good as using one of the
> cooking oils but I avoid the best I can breathing the fumes from
> quenching. It is much cleaner than used motor oil with much lower
> additive package. I use a 15 gallon beer keg for my quench container so I
> have about 14 gallons in the keg. The top was cut out and I have a
> fabricated lid to drop in place in case of fire.
>
> Most likely the best quench oil are the commercial ones -- cost is around
> $ 80 for 5 gallons. Some of the knife maker supply houses sell these
> oils. I know of no industrial heat treaters that use cooling oil for
> quenching.
>
> One note of special care with quench oil -- you can collect water in the
> bottom of your container and never know it -- from say storing your
> contain outside of the shop and collecting rain. If you drop by mistake
> hot metal into such a container you can cause the water in the bottom to
> boil and blow oil out of the contain in one big burp. Makes for a mess,
> and serious fire risk.
>
> Dave
> ----- Original Message -----
> From: "lee robbins" <naturadoc1 at yahoo.com>
> To: <theforge at mailman.qth.net>
> Sent: Monday, November 12, 2007 10:37 AM
> Subject: [TheForge] new question, quenching oil
>
>
>> has anyone had any experienced quenching oil hardening
>> steel in hydraulic oil. i emptied my backhoe after
>> draining the system to fix a pipe and added fresh oil
>> and the old stuff seems perfect. I wonder if anyone
>> has had experience with this and if there is any
>> reason to avoid it.
>>
>> Lee Robbins
>> Flying tortoise forge studio
>>
>> __________________________________________________
>> Do You Yahoo!?
>> Tired of spam? Yahoo! Mail has the best spam protection around
>> http://mail.yahoo.com
>> _______________________________________________
>> Manage membership or unsubscribe at:
>> http://mailman.qth.net/mailman/listinfo/theforge
>> theforge mail list group photo site is
>> http://www.photoaccess.com
>> Login: blacksmithblacksmith at hotmail.com
>> password: anvil
>> ___________
>>
>>
>>
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
>
More information about the TheForge
mailing list