[TheForge] Swage block stands

Roger R Degner rog781 at means.net
Tue Jun 19 21:20:50 EDT 2007


Seen pictures of stands made from angle iron
Sat in frame when flat and had a dropped center frame to allow it to sit
there on edge at the same height as when flat

Not sure if there are pictures at www.iforgeiron.com in the blue print
section but there are a lot of nice plans there with plenty of pictures.
Hoffi put hundred pictures or more.

Roger R Degner


I have one of those swage blocks that doesn't have the rotating ends on. I
was think of welding up a stand from old bed rails, anyone have any ideas of
doing this sort thing?

Jerry