Another purpose of the stone is to have something that stores heat.  As the 
stone heats up, it stores more heat than a metal pan.  When I am baking, the 
top is often brown before the inside is cooked.  I can turn off the oven, 
but leave the bread on the stone (in my case, a thick (3/4 inch) ceramic 
bowl.  The hot stone will continue to cook from below without cooking the 
top of the bread.

Danr
----- Original Message ----- 
From: "Saint Phlip" <phlip at 99main.com>
To: "Sponsored by ABANA" <theforge at mailman.qth.net>
Sent: Friday, January 19, 2007 9:05 AM
Subject: Re: [TheForge] blacksmith bread OT


> The idea of a baker's stone is two-fold- to provide a smooth surface,
> and to provide one that radiates heat specificly to the bottom of the
> loaf.
>
> Keeping that in mind, I'd want a piece of polished stainless at least
> 1/4" thinck, and probably 3/8". Thicker would work to, but now you're
> getting to the point where you oven racks may not be able to bear the
> weight.
>
> Personally, rather than do that, I'd build a tandoori oven.
>
> On 1/19/07, schade at acegroup.cc <schade at acegroup.cc> wrote:
>>
>> Would a piece of sheet or plate steel heated in the oven serve the same
>> purpose as a bakers stone?
>>
>> How thick? 1/4"?
>>
>> Thanks.
>>
>> Bob
>>
>> _______________________________________________
>> Manage membership or unsubscribe at:
>> http://mailman.qth.net/mailman/listinfo/theforge
>> theforge mail list group photo site is
>> http://www.photoaccess.com
>> Login:  blacksmithblacksmith at hotmail.com
>> password:  anvil
>> ___________
>>
>>
>>
>
>
> -- 
> Saint Phlip
>
> Heat it up
> Hit it hard
> Repent as necessary.
>
> Put not your trust in princes, nor in the son of man, in whom there is no 
> help.
>
> Psalm 146
> King James Bible
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  blacksmithblacksmith at hotmail.com
> password:  anvil
> ___________
>
>
> 




More information about the TheForge mailing list