You run a danger of destroying the gun ($400) cutting with insufficent air.
----- Original Message ----- 
From: <marc3rd at marc3rd.com>
To: "Sponsored by ABANA" <theforge at mailman.qth.net>
Sent: Thursday, February 08, 2007 3:15 AM
Subject: Re: [TheForge] Plasmas


> Mine uses a lot of air. I have limited current to my forge so I have to 
> run the plasma cutter or the compressor. So I charge the compressor (30 
> gal at 125 psi ) and then turn it off and cut. I only get about a minute 
> maybe a minute and a half cutting time. then I have to do it all over 
> again.
> I think they run better or more efficiently on nitrogen, but I have always 
> ran mine on air.
>
> Marc V Davis III
> Marc of the Hammer
> WWW.Marc3rd.com
>
> "It's not about the light you reflect. It's about the light you radiate." 
> M3
>
>
>
> ----- Original Message ----- 
> From: "Justin Fisher" <justinf at pixelations.com>
> To: "Sponsored by ABANA" <theforge at mailman.qth.net>
> Sent: Wednesday, February 07, 2007 7:55 PM
> Subject: Re: [TheForge] Plasmas
>
>
>> Bruce wrote:
>>
>> I don't know much about plasma cutters, but I don't think they use all 
>> that
>> much air.  (In fact, I thought they used nitrogen, not air.  But whaddo I 
>> know?)
>> ----------------------------------------------------------------------------
>>
>> I've got a little plasma unit with a built in compressor - not much air 
>> volume at all, really.  Since air is mostly nitrogen, it's about the same 
>> thing I imagine.  The oxygen in air probably has an effect, but it hasn't 
>> given me any trouble.
>>
>> --Justin
>> _______________________________________________
>> Manage membership or unsubscribe at:
>> http://mailman.qth.net/mailman/listinfo/theforge
>> theforge mail list group photo site is
>> http://www.photoaccess.com
>> Login:  blacksmithblacksmith at hotmail.com
>> password:  anvil
>> ___________
>>
>>
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  blacksmithblacksmith at hotmail.com
> password:  anvil
> ___________
>
>
> 




More information about the TheForge mailing list