[TheForge] Plasmas
marc3rd at marc3rd.com
marc3rd at marc3rd.com
Thu Feb 8 09:52:14 EST 2007
Yea I know. That's why I only get a minute of cutting. It has an auto cut
off but I usually stop about 10 - 20 lbs before it.
----- Original Message -----
From: "Dan Tull" <dantull at numail.org>
To: <marc3rd at marc3rd.com>; "Sponsored by ABANA" <theforge at mailman.qth.net>
Sent: Thursday, February 08, 2007 9:44 AM
Subject: Re: [TheForge] Plasmas
> You run a danger of destroying the gun ($400) cutting with insufficent
> air.
> ----- Original Message -----
> From: <marc3rd at marc3rd.com>
> To: "Sponsored by ABANA" <theforge at mailman.qth.net>
> Sent: Thursday, February 08, 2007 3:15 AM
> Subject: Re: [TheForge] Plasmas
>
>
>> Mine uses a lot of air. I have limited current to my forge so I have to
>> run the plasma cutter or the compressor. So I charge the compressor (30
>> gal at 125 psi ) and then turn it off and cut. I only get about a minute
>> maybe a minute and a half cutting time. then I have to do it all over
>> again.
>> I think they run better or more efficiently on nitrogen, but I have
>> always ran mine on air.
>>
>> Marc V Davis III
>> Marc of the Hammer
>> WWW.Marc3rd.com
>>
>> "It's not about the light you reflect. It's about the light you radiate."
>> M3
>>
>>
>>
>> ----- Original Message -----
>> From: "Justin Fisher" <justinf at pixelations.com>
>> To: "Sponsored by ABANA" <theforge at mailman.qth.net>
>> Sent: Wednesday, February 07, 2007 7:55 PM
>> Subject: Re: [TheForge] Plasmas
>>
>>
>>> Bruce wrote:
>>>
>>> I don't know much about plasma cutters, but I don't think they use all
>>> that
>>> much air. (In fact, I thought they used nitrogen, not air. But whaddo
>>> I know?)
>>> ----------------------------------------------------------------------------
>>>
>>> I've got a little plasma unit with a built in compressor - not much air
>>> volume at all, really. Since air is mostly nitrogen, it's about the
>>> same thing I imagine. The oxygen in air probably has an effect, but it
>>> hasn't given me any trouble.
>>>
>>> --Justin
>>> _______________________________________________
>>> Manage membership or unsubscribe at:
>>> http://mailman.qth.net/mailman/listinfo/theforge
>>> theforge mail list group photo site is
>>> http://www.photoaccess.com
>>> Login: blacksmithblacksmith at hotmail.com
>>> password: anvil
>>> ___________
>>>
>>>
>>
>> _______________________________________________
>> Manage membership or unsubscribe at:
>> http://mailman.qth.net/mailman/listinfo/theforge
>> theforge mail list group photo site is
>> http://www.photoaccess.com
>> Login: blacksmithblacksmith at hotmail.com
>> password: anvil
>> ___________
>>
>>
>>
>
>
> _______________________________________________
> Manage membership or unsubscribe at:
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: blacksmithblacksmith at hotmail.com
> password: anvil
> ___________
>
>
More information about the TheForge
mailing list